Inspection Key Points for Bus Automotive Glass
Appearance : Check for stones, bubbles, foreign inclusions, scratches, edge chipping, water marks and printing ink defects. Optical performance : For front windshields, inspect optical distortion and
Explore the journal
Appearance : Check for stones, bubbles, foreign inclusions, scratches, edge chipping, water marks and printing ink defects. Optical performance : For front windshields, inspect optical distortion and
Bus glass includes laminated heat‑bent front windshields, tempered side‑window glass, emergency break‑out windows, sliding movable windows and rear‑window glass. It shall comply with the national stan
People who often ride in cars may notice a small detail, a small black dot around the edge of the windshield. Many people believe that this is a manufacturer's sticker and do not remove it horizontall
1. Ingredients, according to the designed material list, weigh various materials and mix them evenly in a mixer. The primary materials for glass include quartz sand, limestone, feldspar, soda ash, bor
Visual Inspection 100% inspection on transparent surfaces: no scratches, pits, stones, air bubbles or stains; no white fog or delamination on laminated glass; no missing printing or ink peeling on sil
1、 Mixing uncertified raw glass, recycled glass, inferior PVB film or printing ink is strictly prohibited, as this will directly result in the invalidation of the 3C certification qualification. 2、Def
Impact resistant and durable Suitable for high-speed impact of crushed stones, straw, and tree branches in the field, resistant to long-term bumps and vibrations of agricultural machinery, and not eas
Performance characteristics 1. Tempered agricultural machinery glass (mainly for side windows, door glass, and rear windows) -The impact resistance strength is 3-5 times that of ordinary glass, and af
1. Laminated tempered glass (standard for front windshield) Structure: Double layer tempered glass+middle PVB film Core advantage: After being hit by gravel or overturned, the fragments stick to the a
Performance characteristics 1. Safety performance After physical tempering, the strength is 3-5 times that of ordinary float glass; After crushing, it forms obtuse angle particles without sharp fragme
Scroll down to load more.
Load moreProduct Inquiry